Sasany, Rafat; Donmez, Mustafa Borga; de Paula, Marcella Silva; Kahveci, Çiğdem; Ceylan, Gözlem; Yilmaz, Burak; Çakmak, Gülce (2024). Stainability and translucency of potassium aluminum sulfate applied computer-aided design and computer-aided manufacturing materials after coffee thermocycling. Journal of esthetic and restorative dentistry, 36(3), pp. 477-483. Wiley 10.1111/jerd.13154
|
Text
J_Esthet_Restor_Dent_-_2023_-_Sasany_-_Stainability_and_translucency_of_potassium_aluminum_sulfate_applied_computer_aided.pdf - Published Version Available under License Creative Commons: Attribution (CC-BY). Download (573kB) | Preview |
OBJECTIVE
The purpose of this in vitro study was to evaluate the effect of potassium aluminum sulfate (alum) application on the stainability and translucency of computer-aided design and computer-aided manufacturing (CAD-CAM) materials after coffee thermocycling (CTC).
MATERIALS AND METHODS
Disk-shaped specimens (Ø10 × 1 mm; N = 200) were fabricated by using additively (Crowntec [CT] and Varseo Smile Crown Plus [VS]) and subtractively manufactured (Brilliant Crios [RCR], CEREC Block [FC], and Vita Enamic [VE]) CAD-CAM materials and polished. All specimens were randomly divided into two groups as alum applied and control (n = 10). All specimens were then subjected to CTC (10,000 cycles at 5-55°C) and color coordinates were measured at each time interval. Color differences (ΔE00 ) and relative translucency parameters (RTPs) were calculated and the data were statistically analyzed (a = 0.05).
RESULTS
Among tested time intervals, alum applied specimens had their lowest ΔE00 after alum application (p ≤ 0.006), except for FC (p = 0.177). In addition, alum applied RCR had lower ΔE00 values than its control specimens (p = 0.029). Alum applied specimens had their lowest RTP after CTC (p < 0.001) and alum application decreased the RTP of CT (p = 0.010). CTC reduced the RTP of all materials in control groups (p < 0.001). Alum applied CT had higher RTP than its control specimens (p = 0.049).
CONCLUSIONS
Alum application's effect on color change varied depending on the material and alum mostly resulted in clinically acceptable changes in translucency. CTC led to unacceptable color and translucency changes based on previously reported threshold values.
CLINICAL SIGNIFICANCE
Optical properties of CAD-CAM materials and the sustainability of these properties over time is critical for longevity. Alum may improve the color stability of reinforced composite resin when subjected to long-term coffee consumption.
Item Type: |
Journal Article (Original Article) |
---|---|
Division/Institute: |
04 Faculty of Medicine > School of Dental Medicine > Department of Preventive, Restorative and Pediatric Dentistry 04 Faculty of Medicine > School of Dental Medicine > Department of Reconstructive Dentistry and Gerodontology 04 Faculty of Medicine > School of Dental Medicine |
UniBE Contributor: |
Dönmez, Mustafa-Borga, Yilmaz, Burak, Cakmak, Gülce |
Subjects: |
600 Technology > 610 Medicine & health |
ISSN: |
1708-8240 |
Publisher: |
Wiley |
Language: |
English |
Submitter: |
Pubmed Import |
Date Deposited: |
26 Oct 2023 10:05 |
Last Modified: |
18 Feb 2024 00:13 |
Publisher DOI: |
10.1111/jerd.13154 |
PubMed ID: |
37877244 |
Uncontrolled Keywords: |
CAD-CAM coffee thermocycling potassium aluminum sulfate stainability translucency |
BORIS DOI: |
10.48350/187444 |
URI: |
https://boris.unibe.ch/id/eprint/187444 |